Zhu SW, Shi WF (2003c) Thermal degradation of a new flame retardant phosphate methacrylate polymer. Polymer Degradation and Stability 80(2), 217-222. [In English]

Web link: http://dx.doi.org/10.1016/s0141-3910(02)00401-9

Keywords:

phosphate, thermal degradation, flame retardant, amorphous-carbon films, spectroscopy, xps, mechanisms, graphite, surface, resins, ftir,

Abstract: The thermal degradation of a phosphate methacrylate polymer was monitored by in-situ FTIR, XPS, XRD and Raman measurements to investigate the variation in chemical structure and element contents, as well as the carbon structure of the final char formed after burning. The results show that the phosphate group decomposes easily in the range 200-250 degreesC. The degraded products further react with aromatic polynuclear hydrocarbons, formed above 270 degreesC to give phosphorus-carbon complexes. These complexes finally condense to form a graphite-like structure with an interplanar distance of 3.62Angstrom. (C) 2003 Elsevier Science Ltd. All rights reserved.

 
Print    Close
 
 
   
  
 
Relevant link
Contact us
State Key Laboratory of Fire Science, University of Science and Technology of China
Jinzhai Road 96, Hefei, Anhui, P. R. China
P. O.: 230026
   
Tel:(+86)551 63601651
Fax:(+86)551 63601669
E-mail:sklfs@ustc.edu.cn
 
 
Copyright © 1990-2011 State Key Laboratory of Fire Science, University of Science and Technology of China
Tel:(+86)551 3601651 | Fax:(+86)551 3601669 | E-mail:sklfs@ustc.edu.cn | ICP: D20380176