X. M. Feng, B. B. Wang, X. Wang, P. Y. Wen, W. Cai, Y. Hu and K. M. Liew (2016) Chemical Engineering Journal 295 278-287.
Date: 2017-03-14   Author: SKLFS  ,   Source: SKLFS  ,
 

X. M. Feng, B. B. Wang, X. Wang, P. Y. Wen, W. Cai, Y. Hu and K. M. Liew (2016) Molybdenum disulfide nanosheets as barrier enhancing nanofillers in thermal decomposition of polypropylene composites. Journal/Chemical Engineering Journal 295 278-287. [In English]
Web link: http://dx.doi.org/10.1016/j.cej.2016.03.059
Keywords: ,Molybdenum disulfide nanosheets, Latex technology, Polypropylene, nanocomposites, Thermal stability, Physical barrier effect, MECHANICAL-PROPERTIES, EPOXY COMPOSITES, MOS2 NANOSHEETS, GRAPHENE, OXIDE, LAYER MOS2, NANOCOMPOSITES, STABILITY, FUNCTIONALIZATION, FLAMMABILITY, EXFOLIATION

Abstract: A novel method of preparing the molybdenum disulfide (MoS2) nanosheets coated by polypropylene (PP) latex enables the fabrication of PP/MoS2 nanocomposites in scalable quantities. PP nanocomposites with various contents of MoS2 nanosheets were prepared by simply melt-blending the coated MoS2 and PP materials. The barrier effect of MoS2 nanosheets in the thermal decomposition process of PP materials was investigated under different atmosphere by thermogravimetric analysis (TGA), microscale combustion colorimeter (MCC) and thermogravimetric analysis-infrared spectrometry (TG-IR). Importantly, the peak heat release rate (PHRR) of PP/MoS2 nanocomposites with MoS2 loadings of 1.6 wt% is decreased by 28.1% compared to that of neat PP. Moreover, the thermal oxidative stability of PP is dramatically reinforced with the incorporation of MoS2 nanosheets. A 413 degrees C increase in the temperature of the onset of degradation (T-10%) and a 40.1 degrees C increase in the temperature of maximum weight loss (Tmax) were observed by inclusion of as low as 1.6 wt% MoS2 nanosheets. The excellent barrier performance together with the favorable compatibility of MoS2 nanosheets is regarded as the key point for the reinforcement of thermal oxidative stability and reduction of flammable pyrolysis gas, which can provide promising applications in the development of fire safety polymer materials. (C) 2016 Elsevier B.V. All rights reserved.

 
Print    Close
 
 
   
  
 
Relevant link
Contact us
State Key Laboratory of Fire Science, University of Science and Technology of China
Jinzhai Road 96, Hefei, Anhui, P. R. China
P. O.: 230026
   
Tel:(+86)551 63601651
Fax:(+86)551 63601669
E-mail:sklfs@ustc.edu.cn
 
 
Copyright © 1990-2011 State Key Laboratory of Fire Science, University of Science and Technology of China
Tel:(+86)551 3601651 | Fax:(+86)551 3601669 | E-mail:sklfs@ustc.edu.cn | ICP: D20380176