Wang ZZ, Wu GS, Hu Y, Ding Y, Hu KL, Fan WC (2002d) Polymer Degradation and Stability 77(3), 427-434.
Date: 2011-08-16   Author: SKLFS  ,   Source: WOS  ,
 

Wang ZZ, Wu GS, Hu Y, Ding Y, Hu KL, Fan WC (2002d) Thermal degradation of magnesium hydroxide and red phosphorus flame retarded polyethylene composites. Polymer Degradation and Stability 77(3), 427-434. [In English]

Web link: http://dx.doi.org/10.1016/s0141-3910(02)00099-x

Keywords:

thermal degradation, kinetic analysis, pyrolysis, polyethylene, magnesium hydroxide, red phosphorus, capillary gas-chromatography, copolymers, polymers,

Abstract: The thermal degradation of flame-retarded linear low-density polyethylene (LLDPE) composites containing magnesium hydroxide (MH) and red phosphorus (RP) has been studied by thermogravimetric analysis, real time Fourier transform infrared (FTIR) and pyrolysis gas chromatography mass spectrometry (Py-GC/MS). The Kissinger and Flynn-Wall methods were used to calculate the apparent activation energy (Ea) of the degradation of LLDPE and LLDPE composites. The FTIR studies show that addition of MH to LLDPE improves the thermo-oxidative stability, especially LLDPE/MH composites with suitable amount of RP at higher temperatures. The Py-GC/MS data indicate that incorporation of RP into the LLDPE/MH composite results in a change of pyrolysis mode and thus a great increase of the amounts of compounds with high molecular weights. (C) 2002 Elsevier Science Ltd. All rights reserved.
 
Print    Close
 
 
   
  
 
Relevant link
Contact us
State Key Laboratory of Fire Science, University of Science and Technology of China
Jinzhai Road 96, Hefei, Anhui, P. R. China
P. O.: 230026
   
Tel:(+86)551 63601651
Fax:(+86)551 63601669
E-mail:sklfs@ustc.edu.cn
 
 
Copyright © 1990-2011 State Key Laboratory of Fire Science, University of Science and Technology of China
Tel:(+86)551 3601651 | Fax:(+86)551 3601669 | E-mail:sklfs@ustc.edu.cn | ICP: D20380176