Cai YB, Hu Y, Song L, Tang Y, Yang R, Zhang YP, Chen ZY, Fan WC (2006b) Journal of Applied Polymer Science 99(4), 1320-1327.
Date: 2011-08-17   Author: SKLFS  ,   Source: WOS  ,
 

Cai YB, Hu Y, Song L, Tang Y, Yang R, Zhang YP, Chen ZY, Fan WC (2006b) Flammability and thermal properties of high density polyethylene/paraffin hybrid as a form-stable phase change material. Journal of Applied Polymer Science 99(4), 1320-1327. [In English]

Web link:http://dx.doi.org/10.1002/app.22065

Keywords: ,

phase change material (PCM), flame retardant, heat release rate, latent, heat, layered silicate nanocomposites, red phosphorus, polyphosphate, performance, combustion, retardancy, paraffin, system, clay

Abstract: In this study, form-stable phase change material (PCM)-high density polyethylene (HDPE)/paraffin hybrid with different flame-retardant systems are prepared by using twin-screw extruder technique. This kind of formstable PCM is made up of paraffin (a dispersed phase change material) and a HDPE (a supporting material). Their structures and flammability properties are characterized by scanning electronic microscope (SEM) and cone calorimetry. Thermal stability is shown by thermogravimetry analysis (TGA) and its latent heat is given by differential scanning calorimeter (DSC) method. SEM results show that the HDPE forms a three-dimensional net structure and the paraffin is dispersed in it. The peak of heat release rate (HRR) of the flame-retardant form-stable PCM decreases markedly. In TGA curves, although the onset of weight loss of flame-retardant form-stable PCMs occur at a lower temperature than that of form-stable PCM, flame-retardant form-stable PCMs produce a large amount of char residue at 700 degrees C. DSC results show that the addition of flame retardant has little effect on the phase change latent heat of PCM. (c) 2005 Wiley Periodicals, Inc.

 
Print    Close
 
 
   
  
 
Relevant link
Contact us
State Key Laboratory of Fire Science, University of Science and Technology of China
Jinzhai Road 96, Hefei, Anhui, P. R. China
P. O.: 230026
   
Tel:(+86)551 63601651
Fax:(+86)551 63601669
E-mail:sklfs@ustc.edu.cn
 
 
Copyright © 1990-2011 State Key Laboratory of Fire Science, University of Science and Technology of China
Tel:(+86)551 3601651 | Fax:(+86)551 3601669 | E-mail:sklfs@ustc.edu.cn | ICP: D20380176